Relationship between crystallization behavior, microstructure, and mechanical properties in a palm oil-based shortening
In this study, the effects of cooling rate, degree of supercooling, and storage time on the microstructure and rheological properties of a vegetable shortening composed of soybean and palm oils were examined. The solid fat content vs. temperature profile displayed two distinct regions: from 5 to 25°...
Guardado en:
Autores principales: | , , , |
---|---|
Formato: | JOUR |
Materias: | |
Acceso en línea: | http://hdl.handle.net/20.500.12110/paper_0003021X_v79_n7_p647_Litwinenko |
Aporte de: |
Sumario: | In this study, the effects of cooling rate, degree of supercooling, and storage time on the microstructure and rheological properties of a vegetable shortening composed of soybean and palm oils were examined. The solid fat content vs. temperature profile displayed two distinct regions: from 5 to 25°C, and from 25°C to the end of melt at 45-50°C. A peak melting temperature of 42.7°C was determined by DSC. Discontinuity in the crystallization induction time (determined by pulsed NMR) vs. temperature plot at 27°C also suggested the existence of two separate groups of crystallizing material. Isothermal crystallization kinetics were characterized using the Avrami and Fisher-Turnbull models. In using DSC and powder X-ray diffraction, the α polymorph formed upon fast cooling (>5°C/min), and the β′ form predominated at lower cooling rates (<1°C/min). An α to β′ transition took place upon storage. Fractal dimensions (Df) obtained by microscopy and image analysis showed no dependence on the degree of supercooling since Df remained constant (∼1.89) at crystallization temperatures of 5, 22, and 27°C. Crystallization at 22°C at 1°C/min and 15°C/min yielded Df values of 1.98 and 1.93, respectively. Differences in microstructure were observed, and changes in particle properties increased the parameter λ at higher degrees of supercooling. |
---|