Nickel zinc ferrites prepared by the citrate precursor method

Ni1-xZnxFe2O4 (x = 0.2, 0.4, 0.5, 0.6 and 0.7) were prepared by a combustion method. The precursors for the solids were different gels obtained from metal nitrates and citric acid by a sol-process. The gels thus obtained were heated at 200°C and they exhibited self-propagating combustion behavior. T...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Sileo, E.E., Rotelo, R., Jacobo, S.E.
Formato: JOUR
Materias:
Acceso en línea:http://hdl.handle.net/20.500.12110/paper_09214526_v320_n1-4_p257_Sileo
Aporte de:

Ejemplares similares