Quenching and Partitioning Process in Ductile Cast Irons
A commercial ductile iron alloy was submitted to Quenching and Partitioning (Q&P) process. Samples were austenitized at 900ºC for two hours, quenched at 170ºC and held at this temperature for 2 minutes and finally were re-heated in temperatures between 300 and 450ºC in time intervals between 2 a...
Guardado en:
| Autores principales: | da Silva, A.J.S.T., de Campos, M.F., Nishikawa, A.S., Guesser, W.L., Goldenstein, H. |
|---|---|
| Formato: | Artículo |
| Lenguaje: | Inglés |
| Publicado: |
INTEMA - UNMdP-CONICET
2014
|
| Acceso en línea: | 10 Th International Symposium on the Science and Processing of Cast Iron. 2014. Argentina: Mar del Plata 10 to 13th of November. |
| Aporte de: |
Ejemplares similares
-
A Computational Micromechanics Approach to Evaluate Effective Properties of Ductile Cast Iron
por: Rodriguez, F.J., et al.
Publicado: (2014) -
Ductile iron handbook
por: Alagarsamy, A.
Publicado: (1993) -
Effect of Cu, Mn and Sn on Pearlite Growth Kinetics in as-Cast Ductile Irons
por: Lacaze, J., et al.
Publicado: (2014) -
Numerical Simulation of Dimensional Change During Austempering Heat Treatment in Ductile Cast Iron
por: Boccardo, A.D., et al.
Publicado: (2014) -
Numerical Simulation of Dimensional Change During Austempering Heat Treatment in Ductile Cast Iron
por: Boccardo, A.D., et al.
Publicado: (2014)