Effect of Cooling Rate and of Titanium Additionson the Microstructure of Thin-Walled Compacted Iron Castings
This article addresses the effect of cooling rate and of titanium additions on the exhibited microstructure of thin-walled compacted graphite iron (TWCI) castings as determined by changing molding media, section size and Ferro Titanium. Various molding materials were employed (silica sand and insula...
Guardado en:
| Autores principales: | Górny, M., Kawalec, M., Sikora, G., Lopez, H. |
|---|---|
| Formato: | Other |
| Lenguaje: | Inglés |
| Publicado: |
INTEMA - UNMdP-CONICET
2014
|
| Materias: | |
| Acceso en línea: | http://rinfi.fi.mdp.edu.ar/handle/123456789/38 |
| Aporte de: |
Ejemplares similares
-
Effect of Cooling Rate and of Titanium Additionson the Microstructure of Thin-Walled Compacted Iron Castings
por: Górny, M., et al.
Publicado: (2014) -
The Occurrence and the Effect of Casting Skin in Compacted Graphite Iron
por: Boonmee, S., et al.
Publicado: (2014) -
A Study of the Oxygen Activity Before Start of Solidification of Cast Irons
por: Ekengård, J., et al.
Publicado: (2014) -
Solidification Macrostructure of Compacted Graphite Cast Iron and Its Relationship with Shrinkage Porosity
por: López, M., et al.
Publicado: (2014) -
Understanding Compacted Graphite Iron Solidification through Interrupted Solidification Experiments
por: Alonso, G., et al.
Publicado: (2014)